Stick Welding Basics for Beginners: A Complete 101 Guide

A coated electrode strikes an arc that melts both the rod and the base metal, while its coating shields the molten pool from the air.

Shielded metal arc welding — the process most people just call stick welding — runs on one moving part: the rod. There is no gas bottle, no wire feeder, and no tank to refill. An electric arc jumps between the coated electrode and the steel, melting both into a single pool, and the burning coating does the protective work a shielding-gas cylinder handles on other processes. That single fact explains why stick welders survive in muddy barns, on pipeline right-of-ways, and in windy farmyards where a gas cloud would blow sideways.

What follows is the honest starting sequence: which machine settings matter, why polarity changes the bead, how to run your first arc, and which mistakes send beginners back to the scrap pile.

What Equipment Does Stick Welding Actually Need?

Stick welding requires an AC or DC welder, an electrode holder, a work lead with a clamp, electrodes, and a full set of protective gear. The gear list is short but none of it is optional.

Protection first, because this process throws sparks and ultraviolet light in every direction. Lincoln Electric’s process documentation lists a welding helmet with the correct filter lens, safety glasses with side shields, dry welding gloves, flame-resistant clothing, and nonflammable footwear. Add ventilation or local exhaust — burning electrode coatings produce smoke you should not breathe in a closed garage.

  • Welder — AC, DC, or an AC/DC machine rated for the electrode you plan to run.
  • Electrode holder and work clamp — the clamp must bite clean metal, close to the joint.
  • Chipping hammer and wire brush — slag removal between passes is part of welding, not cleanup.
  • Electrodes — matched to the metal, the position, and your machine’s output.

If you are assembling a first setup, this roundup of tested stick welding equipment picks covers the hardware side in more detail.

Which Electrode Should A Beginner Buy?

E6011 is the friendliest starting point on a small AC machine, and E7018 covers stronger structural joints on machines that will run it well. The digits on the label are not random: in the AWS classification, the first two numbers give minimum tensile strength in ksi, the third gives welding position, and the last two describe coating and current characteristics.

Polarity is where first-timers get burned. Lincoln Electric’s polarity guidance notes that electrode-positive welding generally delivers deeper penetration, while electrode-negative raises melt-off and deposition rate — and the wrong setting shows up as poor fusion, spatter, an unstable arc, and rods that vanish fast.

  • E6010 — vertical-up and overhead work, on electrode-positive polarity, in the lower part of its current range. Lincoln recommends 3/16 inch and smaller rods for those positions.
  • E6011 — the AC substitute for E6010, run at roughly 10% higher current. This is why small AC-only welders ship with it.
  • E7018 — electrode-positive preferred; AC works at about 10% more current on rods 5/32 inch and under. It is low-hydrogen and moisture-sensitive, so store it dry.

Always confirm the exact classification and current range on the label or the manufacturer’s data sheet before striking an arc.

Electrode Polarity and Current Best For
E6010 Electrode-positive, low end of range Vertical-up, overhead, dirty steel
E6011 AC, about 10% more current than E6010 AC-only machines, general repair
E7018 (5/32 in and under) Electrode-positive preferred; AC at +10% Structural joints, low-hydrogen work
Any rod over 3/16 in Per manufacturer range Flat work on high-output machines
Wrong polarity (any rod) Not compatible Nothing — expect spatter and poor fusion
Damp or damaged coating Not compatible Nothing — arc will run rough and porous
Rust, paint, oil, galvanized zinc Clean before welding Nothing — remove it first

How Do You Strike And Hold An Arc?

Strike the arc by briefly touching or scratching the rod against the work, then lift it slightly to hold a short, steady arc. Every beginner step below follows Lincoln Electric’s operating sequence, and skipping any one of them shows up in the bead.

  1. Read the welder and electrode instructions. Confirm the rod diameter, its current range, and whether it permits AC or DC polarity.
  2. Clean rust, paint, oil, moisture, and mill scale from the joint. Lincoln’s process guidance lists welding over these contaminants as a leading cause of bad welds.
  3. Clamp the work securely. Attach the work clamp to clean metal close to the weld area so the work cable makes a solid electrical connection.
  4. Connect the electrode and work leads for the polarity you chose. Positive polarity uses the positive terminal.
  5. Set the amperage inside the rod manufacturer’s range. Start low — you can always add heat, but burn-through cannot be undone.
  6. Practice on scrap before touching a critical joint. Build a row of beads until the arc stays lit.
  7. Hold a consistent travel speed, rod angle, and arc length. Keep the molten pool controlled as you move.
  8. Let the weld cool, then chip the slag and brush it clean before inspecting or running another pass.
  9. Stop immediately if the rod sticks. Break the arc and free the electrode without grabbing hot metal with bare hands.

When the arc holds steady and the rod feeds without sticking, you have it.

What Are The Most Common Beginner Mistakes?

Most failed first beads trace back to four habits: wrong polarity, too long an arc, wrong travel speed, and welding over dirt. Lincoln Electric’s polarity documentation confirms the first — an incorrect setting causes poor penetration, irregular bead shape, excess spatter, an unstable arc, and rods that burn away too fast.

  • Arc too long — more spatter, and a porous or weak bead. Hold the rod closer to the work.
  • Moving too fast — narrow bead without fusion at the edges. Slow down and watch the pool wet out.
  • Moving too slow — excess buildup, burn-through on thin metal, slag trapped in the weld.
  • Skipping slag removal — the next pass traps junk and the weld fails inspection.
  • Bad clamp placement — a weak connection far from the joint makes the arc wander.
  • Damp electrodes — moisture-sensitive rods like E7018 lose their low-hydrogen advantage.

Pick one mistake per practice session and fix it before adding the next. Beads improve faster that way than chasing every flaw at once, and the habit sticks when you move to out-of-position work. Welding safety standards from Lincoln Electric cover the protective side in full.

Common Questions

How thick should the scrap metal be for practice beads?

Start with quarter-inch plate or thicker. Thin sheet burns through quickly while you are learning heat control, and thick scrap lets you run full beads without chasing holes.

Why does my rod keep sticking to the work?

Sticking usually means the amperage is too low for the rod, or you are holding too long a pause at the start. Confirm the current is inside the manufacturer’s range, and strike quickly rather than resting the rod on the plate. Wet or damaged coating makes it worse.

Can I stick weld outside on a windy day?

The coating generates its own shielding gas, so wind cannot blow it away the way it scatters a gas cylinder’s flow. Keep sparks away from dry grass and check local fire rules first.